Scott Keilbey, director of sales for the water tank market at protective coatings manufacturer Tnemec (Kansas City, Missouri, USA), joins Monday's podcast with Mark Thomas, vice president of marketing,
to discuss their company's recently completed 2020 Tank of the Year program.
Topics include the challenges and opportunities involved with the coating of water tanks, both from an asset owner's perspective and for a contractor. Other subjects include a brief review of this year's winners and an overview of why fluoropolymer coating systems are a popular choice for these environments.
Source: Tnemec, www.tnemec.com.