The Fine Art of Predicting Failures Just Before They Occur

When predicting a corrosion failure, ideally the time frame should be of sufficient duration to enable operators to take the appropriate action and eliminate the hazard. Occasionally it happens that a potential failure is predicted just before it actually occurs. This article describes such a situation.

  Download Article PDF