Amine Blush in Epoxy Coatings

Carbonated amine material, often called amine blush, is the reaction product of the amine functional curatives in epoxy paint with carbon dioxide (CO2) and water vapor. This article explains the formation of amine blush and discusses factors controlled by the applicator and those controlled by the paint manufacturer.