I Told You So

Cathodic protection expert John Fitzgerald uses an experience early in his career to illustrate the consequences of not heeding the advice of corrosion professionals when designing and implementing corrosion control systems—many times because of reluctance to bear the expense. Cutting corners to save money up front can lead to unexpected failures and expensive repair and replacement in the future.