Measurement of a Corrosion Inhibitor Through Online Monitoring

Typical repair of reinforced concrete structures showing corrosion damage involves removal of carbonated or chloride-contaminated concrete and subsequent retrofilling with new concrete. Corrosion inhibitors that can be applied by spraying onto the concrete surface are an alternative. These products are relatively new and only limited long-term monitoring results are available. The combination of an inhibitor with monitoring of the corrosion behavior provides evidence of protection. This article describes long-term monitoring results of protected highway gallery columns in the Swiss Alps.